Test item | Material type | Denier | Bursting strength (kPa) | Mesh size | Active ingredient | Estimated AI dose | Treatment method | Manufacturer | WHO status |
---|---|---|---|---|---|---|---|---|---|
Tsara® Boost | Polyethylene | 130 | ≥ 400 | 21 holes/cm2 | Deltamethrin and PBO | 120 mg/m2 of deltamethrin and 440 mg/m2 of PBO | Incorporated | NRS Moon Netting FZE, United Arab Emirates | [67] |
Olyset® Plus | Polyethylene | 150 | ≥ 250 | 6.45 holes/cm2 | Permethrin and PBO | 800 mg/m2 of Permethrin and 400 mg/m2 of PBO | Incorporated | Sumitomo Chemical, Japan | [70] |
Veeralin® | High-Density Polyethylene | 130 | ≥ 350 | 13 holes/cm2 | Alpha-cypermethrin and PBO | 216 mg/m2 of alpha-cypermethrin and 79.2 mg/m2 of PBO | Incorporated | V.K.A Polymers, India | [68] |
MAGNet® | High-Density Polyethylene | 150 | ≥ 450 | 20 holes/cm2 | Alpha-cypermethrin | 261 mg/m2 of alpha-cypermethrin | Incorporated | V.K.A Polymers, India | [71] |